Nimonik 90/UNS N07090
| Alyaj | eleman | C | Si | Mn | S | Ni | Cr | Al | Ti | Fe | Cu | B | Pb | Zr |
| Nimonik 90 | Minimòm | 18.0 | 1.0 | 2.0 | ||||||||||
| Maksimòm | 0.13 | 1.0 | 1.0 | 0.015 | Balans | 21.0 | 2.0 | 3.0 | 1.5 | 0.2 | 0.02 | 0.015 | 0.15 |
| Estati Aolly | Fòs tansyon ChanmMpa Min | Fòs sede RP 0.2Mpa Min | Elongasyon A5 Minimòm% |
| Ssolisyon &presipitasyon | 1175 | 752 | 30 |
| Dansiteg/cm33 | Pwen fizyon℃ |
| 8.18 | 1310~1370 |
Baton, Ba, Fil ak Materyèl Forge- BS HR2, HR501, HR502 ak HR503; SAE AMS 5829
Plak, Fèy ak Bann -BS HR202, AECMA PrEN 2298.
Tiyo ak tib-BS HR402